Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4764A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL 2530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1035-70 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1488G Thermoplastic Elastomer Uses: Flexible Grips; General Purpose; Handles; Household Goods; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1934G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 1581Forms: Pellets Proces.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1949A-55NT Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2550F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2575F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2596C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2635D Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2683B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-4001A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-88-N882-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-89-P808A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2365A Thermoplastic Polyolefin Elastomer Uses: Automotive Applications; Flexible Grips; Gaskets; General Purpose; Industrial Applications; Roof Vents Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injectio.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2519F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2580A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-8730R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Middle Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |