Polymer Property : Sintering Temperature = 1550 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 1550 - 1700 °C
2820 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9212 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Sintering Temperature 1550 - 1650 °C
2820 - 3000 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1550 - 1650 °C
2820 - 3000 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1550 °C
2820 °F
Nabaltec GRANALOX® NM 9216 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1550 - 1650 °C
2820 - 3000 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9510 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1550 - 1700 °C
2820 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9922 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Sintering Temperature 1550 - 1700 °C
2820 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9922 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1550 - 1700 °C
2820 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..