Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 704 °C @Time 57600 sec |
1300 °F @Time 16.0 hour |
Step 1; then furnace cool to step 2 |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Adapter Temperature | 704 °C @Time 57600 sec |
1300 °F @Time 16.0 hour |
Step 1; then furnace cool to step 2 |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Adapter Temperature | 704 °C @Time 57600 sec |
1300 °F @Time 16.0 hour |
Step 1; then furnace cool to step 2 |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Adapter Temperature | 704 °C @Time 57600 sec |
1300 °F @Time 16.0 hour |
Step 1; then furnace cool to step 2 |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Adapter Temperature | 704 °C @Time 57600 sec |
1300 °F @Time 16.0 hour |
Step 1; then furnace cool to step 2 |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Adapter Temperature | 704 °C @Time 57600 sec |
1300 °F @Time 16.0 hour |
Step 1; then furnace cool to step 2 |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |