Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 480 - 720 min @Temperature 80.0 °C |
8.00 - 12.0 hour @Temperature 176 °F |
|
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Cure Time | 480 - 720 min @Temperature 65.6 °C |
8.00 - 12.0 hour @Temperature 150 °F |
|
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy Master Bond Polymer System EP29LPSP is a two component, high performance, modified low temperature heat cured epoxy system specially formulated for cryogenic applications. EP29LPSP is serviceable at.. |
|||
Cure Time | 480 - 720 min @Temperature 25.0 °C |
8.00 - 12.0 hour @Temperature 77.0 °F |
|
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy .. |
|||
Cure Time | 480 - 720 min @Temperature 24.0 °C |
8.00 - 12.0 hour @Temperature 75.2 °F |
demold time |
BCC Products BC 8880 Polyurethane Elastomer Surface Coat BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br.. |