Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 180 min @Temperature 43.3 °C |
3.00 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Cure Time | 180 min @Temperature 23.0 °C |
3.00 hour @Temperature 73.4 °F |
Stainless steel, handling strength |
Permabond LH150 Anaerobic Threadsealant Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up .. |
|||
Cure Time | 180 min @Temperature 23.0 °C |
3.00 hour @Temperature 73.4 °F |
Zinc, working strength |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Cure Time | 180 - 240 min @Temperature 25.0 °C |
3.00 - 4.00 hour @Temperature 77.0 °F |
De-mold Time |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Cure Time | 180 - 360 min @Temperature 23.0 °C |
3.00 - 6.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond MH199 Anaerobic Gasketmaker Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Cure Time | 180 min @Temperature 93.3 °C |
3.00 hour @Temperature 200 °F |
|
Master Bond EP37-3FLF Low Exotherm Highly Flexible Two Component Epoxy Master Bond Polymer System EP37-3FLF is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. The .. |
|||
Cure Time | 180 min @Temperature 23.9 °C |
3.00 hour @Temperature 75.0 °F |
Tack-free Time |
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable .. |
|||
Cure Time | 180 min @Temperature 60.0 °C |
3.00 hour @Temperature 140 °F |
|
Tra-Con Tra-Bond 240-2 Polyurethane Adhesive TRA-BOND 240-2 polyurethane adhesive is a low outgassing polyurethane adhesive which meets the requirements of NASA specification SP-R-0022. Information provided by Tra-Con Inc. |
|||
Cure Time | 180 min @Temperature 75.0 °C |
3.00 hour @Temperature 167 °F |
|
Tra-Con Tra-Bond 724-17 Polyurethane Adhesive TRA-BOND 724-17 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar a.. |
|||
Cure Time | 180 min @Temperature 75.0 °C |
3.00 hour @Temperature 167 °F |
|
Tra-Con Tra-Bond 724-17GR Polyurethane Adhesive TRA-BOND 724-17GR premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar.. |
|||
Cure Time | 180 min @Temperature 74.0 °C |
3.00 hour @Temperature 165 °F |
preferred |
Tra-Con Tra-Bond 724-5 Low Viscosity Polyurethane Adhesive TRA-BOND 724-5 is a premixed and frozen, electrically insulating, polyurethane adhesive. This resilient adhesive exhibits good adhesion to a wide variety of substrates, including aluminum, solder, n.. |
|||
Cure Time | 180 min @Temperature 70.0 °C |
3.00 hour @Temperature 158 °F |
|
Tra-Con Tra-Bond 9349J Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349J epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349J is excellent for bonding many metals and woods, most plastics.. |
|||
Cure Time | 180 min @Temperature 70.0 °C |
3.00 hour @Temperature 158 °F |
|
Tra-Con Tra-Bond 9349K Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349K epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349K is excellent for bonding many metals and woods, most plastics.. |
|||
Cure Time | 180 min @Temperature 93.3 °C |
3.00 hour @Temperature 200 °F |
|
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
Cure Time | 180 - 240 min @Temperature 93.3 °C |
3.00 - 4.00 hour @Temperature 200 °F |
|
Master Bond EP34AO Epoxy Compound Withstands High Temperatures Description: Master Bond Polymer System EP34AO is a room temperature curing, two component epoxy compound for high temperature bonding and sealing applications especially where thermal conductivity .. |
|||
Cure Time | 180 - 240 min @Temperature 65.6 - 93.3 °C |
3.00 - 4.00 hour @Temperature 150 - 200 °F |
|
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
Cure Time | 180 min @Temperature 70.0 °C |
3.00 hour @Temperature 158 °F |
|
Tra-Con Tra-Bond 9349 Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349 epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349 is excellent for bonding many metals and woods, most plastics a.. |
|||
Cure Time | 180 min @Temperature 16.0 °C |
3.00 hour @Temperature 60.8 °F |
Tack Free |
Chesterton ARC 10 Paste grade machinable composite Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag.. |
|||
Cure Time | 180 min @Temperature 16.0 °C |
3.00 hour @Temperature 60.8 °F |
Tack Free |
Chesterton MRS S2 Metal Rebuilding System An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is.. |
|||
Cure Time | 180 - 300 min @Temperature 60.0 °C |
3.00 - 5.00 hour @Temperature 140 °F |
|
Cytec (Conap) FR-1272 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Cure Time | 180 - 300 min @Temperature 60.0 °C |
3.00 - 5.00 hour @Temperature 140 °F |
|
Cytec (Conap) FR-1274 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Cure Time | 180 min @Temperature 60.0 °C |
3.00 hour @Temperature 140 °F |
|
Cytec Conathane® CC-1155 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Cure Time | 180 min @Temperature 60.0 °C |
3.00 hour @Temperature 140 °F |
|
Cytec Conathane® CE-1175 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Cure Time | 180 min @Temperature 80.0 °C |
3.00 hour @Temperature 176 °F |
|
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |
|||
Cure Time | 180 min @Temperature 16.0 °C |
3.00 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton MRS 5 Metal Rebuilding System MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we.. |
|||
Cure Time | 180 min @Temperature 75.0 °C |
3.00 hour @Temperature 167 °F |
|
Tra-Con Tra-Bond 724-17GR1B3 Polyurethane Adhesive TRA-BOND 724-17GR1B3 premixed and frozen polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, myl.. |
|||
Cure Time | 180 min @Temperature 23.0 °C |
3.00 hour @Temperature 73.4 °F |
Zinc, working strength |
Permabond A1044 Anaerobic Threadsealant Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal.. |