Processing Properties Metric English Comments
Cure Time 42.0 min

@Temperature 140 °C
0.700 hour

@Temperature 284 °F
Trelleborg Emerson & Cuming Eccobond® 930-09 Low Temperature Performance Lighting Epoxy Adhesive
Emerson & Cuming 930-09 Eccobond® Low Temperature Performance Lighting Epoxy AdhesiveFlexible, non-blushing, epoxy adhesive for glass headlamp bonding. Maintains flexibility at temperatures as low ..
Cure Time 42.0 min

@Temperature 200 °C
0.700 hour

@Temperature 392 °F
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive
AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive ..
Cure Time 42.0 min

@Temperature 200 °C
0.700 hour

@Temperature 392 °F
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive
AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati..