Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.00000 min @Temperature 175 °C |
0.1666667 hour @Temperature 347 °F |
|
Momentive Performance Materials LVG342 Low Volatile Silicone Adhesive, Mixed, White LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for.. |
|||
Cure Time | 10.00000 min @Temperature 175 °C |
0.1666667 hour @Temperature 347 °F |
|
Momentive Performance Materials LVG342B Low Volatile Silicone Adhesive Component, Clear LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for.. |
|||
Cure Time | 10.00000 min @Temperature 175 °C |
0.1666667 hour @Temperature 347 °F |
|
Momentive Performance Materials LVG342A Low Volatile Silicone Adhesive Component, White LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for.. |
|||
Cure Time | 10.00000 min @Temperature 100 °C |
0.1666667 hour @Temperature 212 °F |
|
ACC QGel 301 QSI Quantum Silicones High Strength Gel QGel 301 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide.. |
|||
Cure Time | 10.00000 min @Temperature 100 °C |
0.1666667 hour @Temperature 212 °F |
|
ACC QGel 311 QSI Quantum Silicones General Purpose Silicone Gel QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |
|||
Cure Time | 10.00000 min @Temperature 150 °C |
0.1666667 hour @Temperature 302 °F |
|
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par.. |