Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 7.02 min @Temperature 23.0 °C |
0.117 hour @Temperature 73.4 °F |
Zinc, handling strength |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Cure Time | 7.02 min @Temperature 23.0 °C |
0.117 hour @Temperature 73.4 °F |
Zinc, handling strength |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Cure Time | 7.02 min @Temperature 23.0 °C |
0.117 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond LM113 Anaerobic Threadlocker Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 160 °C |
0.117 hour @Temperature 320 °F |
|
Uniseal BETABRACE™ 85001 Epoxy BETABRACE™ 85001 is a composite used for reinforcing sheet metal. It is composed of a moderate temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85001 provides .. |
|||
Cure Time | 7.00 min @Temperature 130 °C |
0.117 hour @Temperature 266 °F |
|
Tra-Con Tra-Bond 526M03 Fast Cure Epoxy Adhesive TRA-BOND 526M03 is a fast cure, high viscosity, two-component epoxy formulation. It develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that incl.. |
|||
Cure Time | 7.00 min @Temperature 125 °C |
0.117 hour @Temperature 257 °F |
|
Tra-Con Tra-Bond FS437 Low Viscosity High Impact Epoxy Adhesive TRA-BOND FS437 is a two-part, low viscosity material formulated for optical applications which require excellent wicking, visible color and high strength. This material has been used successfully fo.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 177 °C |
0.117 hour @Temperature 351 °F |
|
3M Scotchcast™ 260 8 G Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Cure Time | 7.02 min @Temperature 23.0 °C |
0.117 hour @Temperature 73.4 °F |
Zinc, handling strength |
Permabond HM135 Anaerobic Retainer Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras.. |
|||
Cure Time | 7.02 min @Temperature 23.0 °C |
0.117 hour @Temperature 73.4 °F |
Zinc, handling strength |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
Cure Time | 7.02 min @Temperature 23.0 °C |
0.117 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |