Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | <= 1.98 min @Temperature 150 °C |
<= 0.0330 hour @Temperature 302 °F |
touch dry |
Gwent Electronic Materials C2021031D2 Electrode Ink Electrode Ink C2021031D2 is a Silver Palladium (85/15) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Cure Time | <= 1.98 min @Temperature 150 °C |
<= 0.0330 hour @Temperature 302 °F |
touch dry |
Gwent Electronic Materials C2021031D3 Electrode Ink Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |