Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2880 - 10080 min @Temperature 20.0 °C |
48.0 - 168.0 hour @Temperature 68.0 °F |
(2-7 Days) |
Abatron AboCast 8005-6/AboCure 8005-6 Epoxy AboCast 8005-6 is a tan, viscous filled liquid resin with a weight of approximately 11 lbs/gallon. AboCure 8005-6 is an amber, viscous liquid converter with a weight of approximately 10 lbs/gallon. .. |
|||
Cure Time | 7200 - 10080 min @Temperature 15.556 - 26.667 °C |
120 - 168.0 hour @Temperature 60.001 - 80.001 °F |
(5-7 Days) |
Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound AboTar 8101-8 is a 2-part tar-epoxy variable-ratio system. It is weather- and water-proof, flexible, and acid, alkali, and fuel resistant. It can be used neat or with sand or aggregates. Uses: Resu.. |
|||
Cure Time | 7200 - 10080 min @Temperature 24.0 °C |
120 - 168.0 hour @Temperature 75.2 °F |
full cure |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |
|||
Cure Time | 7200 - 10080 min @Temperature 24.0 °C |
120 - 168.0 hour @Temperature 75.2 °F |
complete cure |
BCC Products BC 8880 Polyurethane Elastomer Surface Coat BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br.. |