Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 76.02 min @Temperature 29.0 °C |
1.267 hour @Temperature 84.2 °F |
Tack Free with MEK |
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres.. |