Processing Properties Metric English Comments
Cure Time 18.0 min

@Temperature 22.0 °C
0.300 hour

@Temperature 71.6 °F
50% RH; Handling Time
Parker Chomerics CHO-FORM 5526 EMI Shielding Material
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Cure Time 18.0 min

@Temperature 22.0 °C
0.300 hour

@Temperature 71.6 °F
50% RH, Tack Free Time
Parker Chomerics ParPHorm® 1800 Non-Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Cure Time 18.0 - 40.2 min

@Temperature 80.0 - 100 °C
0.300 - 0.670 hour

@Temperature 176 - 212 °F
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Cure Time 18.0 min

@Temperature 90.0 °C
0.300 hour

@Temperature 194 °F
Trelleborg Emerson & Cuming Eccobond® 927-10 E Needle Bonding Epoxy Adhesive
Emerson & Cuming 927-10 E Eccobond® Needle Bonding Epoxy AdhesiveOne component, fast curing, epoxy adhesive for needle bonding with polypropylene hubs. Also recommended for bonding sealing or insul..
Cure Time 18.0 min

@Temperature 120 °C
0.300 hour

@Temperature 248 °F
Trelleborg Emerson & Cuming Eccobond® A 316 Filler End Cap Epoxy Adhesive
Emerson & Cuming A 316 Eccobond® Filler End Cap Epoxy AdhesiveOne component, pourable, fast heat curing, epoxy adhesive. Exhibits excellent thermal stability and resistance to chemicals. Used as en..
Cure Time 18.0 min

@Temperature 22.0 °C
0.300 hour

@Temperature 71.6 °F
50% RH; Tack Free Time
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Cure Time 18.0 min

@Temperature 22.0 °C
0.300 hour

@Temperature 71.6 °F
50% RH; Tack Free Time
Parker Chomerics CHO-FORM 5531 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed..
Cure Time 18.0 min

@Temperature 22.0 °C
0.300 hour

@Temperature 71.6 °F
50% RH; Tack Free Time
Parker Chomerics CHO-FORM 5538 Conductive Form-In-Place Gaskets
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Copyright © lookpolymers.com All Rights Reserved