Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 150 min @Temperature 121 °C |
2.50 hour @Temperature 250 °F |
|
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Cure Time | 150 min @Temperature 121 °C |
2.50 hour @Temperature 250 °F |
|
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem.. |
|||
Cure Time | 150 min @Temperature 32.0 °C |
2.50 hour @Temperature 89.6 °F |
Light Load |
Chesterton ARC 10 Paste grade machinable composite Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag.. |
|||
Cure Time | 150 min @Temperature 32.0 °C |
2.50 hour @Temperature 89.6 °F |
Light Load |
Chesterton ARC 858 Abrasion resistant rebuilding and faring composite An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 0.15 mm (60 mils) or m.. |
|||
Cure Time | 150 min @Temperature 32.0 °C |
2.50 hour @Temperature 89.6 °F |
Light Load |
Chesterton ARC MX1 Vertical Build Extreme Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”).. |
|||
Cure Time | 150 min @Temperature 16.0 °C |
2.50 hour @Temperature 60.8 °F |
Foot Traffic |
Chesterton ARC NVE SYSTEM Vinyl Ester Lining Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i.. |
|||
Cure Time | 150 min @Temperature 32.0 °C |
2.50 hour @Temperature 89.6 °F |
Light Load |
Chesterton ARC MXC Castable Extreme Wear Compound Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro.. |
|||
Cure Time | 150 min @Temperature 160 °C |
2.50 hour @Temperature 320 °F |
|
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Cure Time | 150 min @Temperature 160 °C |
2.50 hour @Temperature 320 °F |
|
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Cure Time | 150 min @Temperature 16.0 °C |
2.50 hour @Temperature 60.8 °F |
Foot Traffic |
Chesterton ARC NVE VC Vinyl Ester Sealer Description: ARC NVE VC (Veil Coat) is a two-component, modified epoxy novolac vinyl ester sealer coat formulated for application by brush, roller or spray at 0.15-0.25 mm (0.07-0.010”) wet film th.. |
|||
Cure Time | 150 min @Temperature 32.0 °C |
2.50 hour @Temperature 89.6 °F |
Light Load |
Chesterton MRS 10 Metal Rebuilding System Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10.. |
|||
Cure Time | 150 min @Temperature 32.0 °C |
2.50 hour @Temperature 89.6 °F |
Light Load |
Chesterton MRS 58 Metal Rebuilding System An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo.. |