Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 140 min @Temperature 10.0 °C |
2.33 hour @Temperature 50.0 °F |
Tack Free without MEK |
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres.. |