Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HH120 Anaerobic Threadlocker Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for .. |
|||
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HM118 Anaerobic Threadlocker Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s.. |
|||
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HM129 Anaerobic Threadlocker Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st.. |
|||
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HM161 Anaerobic Retaining Compound Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz.. |
|||
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Cure Time | 10.2 min @Temperature 23.0 °C |
0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |