Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C10903P14 Carbon/Graphite Ink Carbon Graphite Ink is used for screen printing working electrodes. This is a carbon graphite ink, which has been optimized to give superior electrochemical performance with good reversibility when.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2000215D3 Silver / Silver Chloride Paste C2000215D3 has a ratio of Silver to Silver Chloride of 80/20. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2000218D5 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 90/10. It is specifically designed to give good adhesion to ceramic substrates. Applications in medical diagnostics, environm.. |
|||
Cure Time | 10.0 min @Temperature 130 °C |
0.167 hour @Temperature 266 °F |
box oven |
Gwent Electronic Materials C2050712D58 Silver Ink for ITO Substrates This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Inks containing these polymers combine excellent chemical, environmental a.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2080110D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. This is has been designed for fine line printing.Screen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Cure Time | 10.0 min @Temperature 130 °C |
0.167 hour @Temperature 266 °F |
box oven |
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e.. |
|||
Cure Time | 10.0 min @Temperature 120 °C |
0.167 hour @Temperature 248 °F |
Press Cure |
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Cure Time | 10.0 min @Temperature 65.0 °C |
0.167 hour @Temperature 149 °F |
|
Tra-Con Tra-Bond 224-1 Rapid Room Temperature Cure Epoxy Adhesive TRA-BOND 224-1 room temperature curing epoxy adhesive develops structural strength rapidly. Unlike most "rapid cure" epoxies which gel in one or two minutes, TRA-BOND 224-1 adhesive exhibits a 30 mi.. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra.. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353.. |
|||
Cure Time | 10.0 min @Temperature 150 °C |
0.167 hour @Temperature 302 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i.. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 360 Low Viscosity Optical Epoxy Adhesive Product Description: EPO-TEK® 360 is a two component, high-temperature grade epoxy for semiconductor, electronics, fiber optics and medical applications.Advantages & Application Notes: Built in col.. |
|||
Cure Time | 10.0 min @Temperature 120 °C |
0.167 hour @Temperature 248 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, .. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
minimum |
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing.. |
|||
Cure Time | 10.0 min @Temperature 150 °C |
0.167 hour @Temperature 302 °F |
|
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Cure Time | 10.0 min @Temperature 75.0 °C |
0.167 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings High Performance Acrylic Topcoat BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is a water dispersible acrylic enamel. HIGH PERFORMANCE ACRYLIC TOPCOAT is designed to be a low VOC and EPA compliant coating with excellent cove.. |
|||
Cure Time | 10.0 min @Temperature 93.3 °C |
0.167 hour @Temperature 200 °F |
Step 1, preceeded by >10 min. air set |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Cure Time | 10.0 min @Temperature 75.0 °C |
0.167 hour @Temperature 167 °F |
Dust Free, at 50% humidity |
Blue River Coatings Primer Sealer-PSWP BLUE RIVER COATINGS PRIMER SEALER-PSWP is a high quality, single component primer formulated specifically for priming wood, vinyl, and most plastic substrates. Performance obtained is equal or super.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2060602D1 Membrane Touch Switch Paste The ink should be gently stirred before use avoiding introduction of air bubbles. It is a polymer based system for printing on polyester, PVC, etc.Can be used in membrane touch switch applicationsSc.. |
|||
Cure Time | 10.0 min @Temperature 75.0 °C |
0.167 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as.. |
|||
Cure Time | 10.0 min @Temperature 130 °C |
0.167 hour @Temperature 266 °F |
box oven |
Gwent Electronic Materials R2070613P2 Resin Binder This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. Phosphor Inks containing these polymers combine excellent chemical, environmental w.. |