Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.80 - 3.00 min @Temperature 149 °C |
0.0300 - 0.0500 hour @Temperature 300 °F |
|
Master Bond EP17HT-3 One component, snap-curing epoxy system Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p.. |