Polymer Property : Hold Pressure = 17400 psi
Polymer Property :
Hold Pressure =
17400 psi
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Hold Pressure
60.0
-
120
MPa
8700
-
17400
psi
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black
Information provided by Eurotec®