Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ Electro 242-15 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability) LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6050 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6071 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2010 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2060 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2670 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2735/30 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2750 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3285/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/60 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT 3719 Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating / USP Class VI Compliancy - Physical Properties are subject to the substrate that is used. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT HE Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating - Physical Properties are subject to the substrate that is used. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/70 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |