Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB7 GR15 NL RT PBT, 15% glass fiber reinforced, PTFE modified, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP10 GR30 NL PPCP, 30% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP10 GR10 NL PPCP, 10% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |