Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F22-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene, Black Applications: Support ductsHousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4650-01UV Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P100-00 Polypropylene, Natural Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F24-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Head lamp housingsBracketsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |