Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT5100-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G40P100-04UV 40% Glass Fiber Reinforced Polypropylene, UV Stabilized, White Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC10P200-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsRecreational vehicle trim and bumpersInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP514-01 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 5.52 - 8.27 MPa | 800 - 1200 psi | |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC30P100-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |