Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |