Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 75.0 MPa | 10900 psi | |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Conditioned) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Hold Pressure | 75.0 MPa | 10900 psi | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |