Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |