Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Hold Pressure | 5.00 - 40.0 MPa @Time 10.0 - 30.0 sec |
725 - 5800 psi @Time 0.00278 - 0.00833 hour |
|
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7041 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2060 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2070 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2670FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2750 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2760 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2841 Liquid Silicone Rubber - Good Flex Life This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3785/30 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4030 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT 3719 Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating / USP Class VI Compliancy - Physical Properties are subject to the substrate that is used. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT HE Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating - Physical Properties are subject to the substrate that is used. |
|||
Hold Pressure | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/35 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |