Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB30 NL PBT, unfilled, natural, high viscosity, extrusion grade
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 NL IL PBT, impact modified, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP30 NL XC30 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |