Processing Properties | Metric | English | Comments |
---|---|---|---|
Extrusion Rate | 5.50 - 7.50 g/min | 5.50 - 7.50 g/min | |
Parker Chomerics CHO-FORM 5532 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553.. |
|||
Extrusion Rate | 5.50 g/min | 5.50 g/min | |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |