Gel Time 0.066666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 232 °C
0.066666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 450 °F
3M Scotchkote™ 412 Fusion Bonded Epoxy Coating
3M Scotchkote Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to preheated steel..