Polymer Property : Casting Temperature = 1420 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 1320 - 1420 °C
2410 - 2590 °F
Wieland 1751 Wilaform Palladium
Approach-steady palladium alloy for nearly all purposes in decoration manufacturingApplications: casting, chains, laminar decoration, pipes, tubingDental