Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 5 | 250 - 300 °C | 482 - 572 °F | |
Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade Notes: MD21 is a medium viscosity grade of nylon 6, designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a.. |