Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Appeel® 20D855 Ethylene Acrylate DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Appeel® 45D747 Polyolefin Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion.. |
|||
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Bynel® 22E757 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic.. |
|||
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Appeel® 20D784 Ethylene Acrylate Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature .. |
|||
Zone 5 | 285 °C | 545 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 2618 Ethylene Methyl Acrylate Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC.. |