Processing Properties Metric English Comments
Zone 4 338 - 388 °C
640 - 730 °F
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins...
Zone 4 338 - 388 °C
640 - 730 °F
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU)
Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po..