Polymer Property : Zone 4 = 635 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn..
Zone 4 335 - 390 °C
635 - 734 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, ..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s..
Zone 4 335 - 390 °C
635 - 734 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta..
Zone 4 335 - 391 °C
635 - 736 °F
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. ..