Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 230 °C | 446 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS.. |
|||
Zone 4 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Zone 4 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Zone 4 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Zone 4 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o.. |
|||
Zone 4 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Zone 4 | 230 °C | 446 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Zone 4 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Zone 4 | 230 °C | 446 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Zone 4 | 230 - 250 °C | 446 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Zone 4 | 230 - 250 °C | 446 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT HB9255D Ester Type TPE Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Zone 4 | 230 °C | 446 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T65D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
Zone 4 | 230 °C | 446 °F | Injection Molding |
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 4 | 230 °C | 446 °F | Injection Molding |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Zone 4 | 230 °C | 446 °F | Injection Molding |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Zone 4 | 230 °C | 446 °F | Injection Molding |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Zone 4 | 230 - 245 °C | 446 - 473 °F | Head |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 4 | 230 - 245 °C | 446 - 473 °F | Head |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Zone 4 | 230 - 275 °C | 446 - 527 °F | |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |