Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 260 - 310 °C | 500 - 590 °F | |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |