Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 4 | 190 °C | 374 °F | |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Zone 4 | 190 °C | 374 °F | |
Borealis LE0574 Polyethylene LE0574 is a thermoplastic black polyethylene compound, specially designed for strippable semi conductive screen applications. It can be used in thermoplastic form or crosslinked via a grafting proce.. |