Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CAT 10 Polyolefin Catalyst CAT 10 is a high density based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst LV/1 Polyolefin Catalyst LV/1 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst LV/1LR Polyolefin Catalyst LV/1LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or .. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Polyolefin Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam .. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LR Polyolefin Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or .. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/4 Polyolefin Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE) POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 4 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Polidiemme® G/220 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |
|||
Zone 4 | 150 °C | 302 °F | |
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDP.. |