Polymer Property : Processing Temperature = 290 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 143 °C

@Time 7200 sec
290 °F

@Time 2.00 hour
Target Cure Temp
Fibre Glast 3100 Style 7781 Prepreg E-Glass Fiberglass Fabric
Prepreg fabrics are pre-impregnated with an epoxy resin system. As a result, nearly perfect resin content and maximum, repeatable strength properties are attainable. When properly fabricated, parts ..
Processing Temperature 143 °C

@Time 7200 sec
290 °F

@Time 2.00 hour
Target Cure Temp
Fibre Glast 3101 3K, 2x2 Twill Weave Prepreg Carbon Fiber Fabric
Prepreg fabrics are pre-impregnated with an epoxy resin system. As a result, nearly perfect resin content and maximum, repeatable strength properties are attainable. When properly fabricated, parts ..
Processing Temperature 143 °C

@Time 7200 sec
290 °F

@Time 2.00 hour
Target Cure Temp
Fibre Glast 3102 2x2 Twill Weave Prepreg Kevlar Fabric
Prepreg fabrics are pre-impregnated with an epoxy resin system. As a result, nearly perfect resin content and maximum, repeatable strength properties are attainable. When properly fabricated, parts ..