| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 210 - 220 °C | 410 - 428 °F | |
| PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | |
| PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | |
| PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 3 | 190 - 220 °C | 374 - 428 °F | |
| Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | |
| Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | |
| Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | |
| Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
| Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
| Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | |
| Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
| Zone 3 | 200 - 220 °C | 392 - 428 °F | |
| Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||