Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 185 - 210 °C | 365 - 410 °F | |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Zone 3 | 190 - 210 °C | 374 - 410 °F | Extruder |
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for .. |
|||
Zone 3 | 193 - 210 °C | 380 - 410 °F | |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Zone 3 | 193 - 210 °C | 380 - 410 °F | |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Zone 3 | 193 - 210 °C | 380 - 410 °F | |
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm.. |
|||
Zone 3 | 193 - 210 °C | 380 - 410 °F | |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Zone 3 | 193 - 210 °C | 380 - 410 °F | |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Zone 3 | 190 - 210 °C | 374 - 410 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Zone 3 | 190 - 210 °C | 374 - 410 °F | Blow Molding |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil.. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | Injection |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | Injection |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Zone 3 | 193 - 210 °C | 379 - 410 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Zone 3 | 190 - 210 °C | 374 - 410 °F | |
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA.. |