Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 220 - 265 °C | 428 - 509 °F | |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Zone 3 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 3 | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 3 | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Zone 3 | 220 - 230 °C | 428 - 446 °F | Injection |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Oil (ASTM D471 No. 1) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 - 230 °C | 428 - 446 °F | |
Eurostar Starglas FX05032 PE Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar. |
|||
Zone 3 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 3 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 3 | 220 °C | 428 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |