Processing Properties Metric English Comments
Zone 3 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer
Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec..
Zone 3 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Zone 3 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;..
Zone 3 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Zone 3 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Zone 3 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Zone 3 213 °C
415 °F
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by  AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade el..
Zone 3 213 °C
415 °F
AdvanSource Biomaterials ChronoFlex® AL 65D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas..