Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Zone 3 | 210 °C | 410 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,.. |
|||
Zone 3 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Zone 3 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Zone 3 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Zone 3 | 210 - 230 °C | 410 - 446 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro.. |
|||
Zone 3 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 3 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 3 | 210 °C | 410 °F | |
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical propert.. |
|||
Zone 3 | 210 °C | 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T95P Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T95P is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical p.. |
|||
Zone 3 | 210 °C | 410 °F | |
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
Zone 3 | 210 - 230 °C | 410 - 446 °F | |
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Zone 3 | 210 °C | 410 °F | Injection Molding |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 3 | 210 - 260 °C | 410 - 500 °F | |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by.. |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
Zone 3 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 3 | 210 °C | 410 °F | Extrusion Coating |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Zone 3 | 210 °C | 410 °F | Blown Film Coextrusion |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Zone 3 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Zone 3 | 210 °C | 410 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Zone 3 | 210 °C | 410 °F | Metering-zone |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Zone 3 | 210 °C | 410 °F | Extrusion |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 3 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1825 Zinc Ionomer Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp.. |
|||
Zone 3 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |