Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 3 | 193 - 216 °C | 379 - 421 °F | |
Styrolution PS-168M Polystyrene Description: Polystyrene 168M is a high heat, high molecular weight general purpose polystyrene with excellent clarity and high stiffness. Due to its high melt strength and high stiffness. PS-168M i.. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 3 | 193 °C | 379 °F | Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Zone 3 | 193 °C | 379 °F | Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 3 | 193 °C | 379 °F | |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 3 | 193 - 210 °C | 379 - 410 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Zone 3 | 193 - 204 °C | 379 - 399 °F | |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |
|||
Zone 3 | 193 °C | 379 °F | Extrusion |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |
|||
Zone 3 | 193 - 199 °C | 379 - 390 °F | Extrusion |
Lubrizol Estane® 58280 Thermoplastic Polyurethane Type: Estane® 58280 is a polyether-type thermoplastic polyurethane (TPU) compound.Features: High resiliency compound, with unique physical properties such as low tensile and compression set, high r.. |
|||
Zone 3 | 193 °C | 379 °F | Extrusion |
Lubrizol Estane® 58437 Thermoplastic Polyurethane Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi.. |