Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 275 - 290 °C | 527 - 554 °F | |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Zone 3 | 265 - 290 °C | 509 - 554 °F | |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 275 - 290 °C | 527 - 554 °F | |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide R1000 PA66, Injection Molded Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RB004 PA66, 20% Glass Bead Filled, Injection Molded Staramide RB004 is a 20% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 260 - 290 °C | 500 - 554 °F | |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF006S-GY9A121 PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006S-GY9A121 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF007S PA66, 35% Glass Fiber Filled, Injection Molded Staramide RF007S is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar. |
|||
Zone 3 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Euros.. |