Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 175 - 190 °C | 347 - 374 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 3 | 175 - 190 °C | 347 - 374 °F | Injection Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Zone 3 | 175 - 190 °C | 347 - 374 °F | Extrusion Molding |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 175 - 190 °C | 347 - 374 °F | Extrusion Molding |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 175 - 190 °C | 347 - 374 °F | Extrusion Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 175 °C | 347 °F | |
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Zone 3 | 175 °C | 347 °F | Extrusion |
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper.. |
|||
Zone 3 | 175 °C | 347 °F | Extrusion |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Zone 3 | 175 °C | 347 °F | Extrusion |
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane Type: Estane® ALR CL87A is an aliphatic, polycaprolactone-based TPU with a Shore A Durometer of 85-90.Features: Contains a UV package that enhances outdoor weatherability. This high performance re.. |
|||
Zone 3 | 175 °C | 347 °F | Extrusion |
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |
|||
Zone 3 | 175 °C | 347 °F | |
Lubrizol Estane® 54601 Thermoplastic Polyurethane Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in A.. |