Processing Properties Metric English Comments
Zone 2 180 °C
356 °F
SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 2 180 °C
356 °F
Extrusion
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane
Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, ..
Zone 2 180 °C
356 °F
Equate EFDC-7050 LLDPE Film Extrusion Resin
EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc..