Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 200 - 225 °C | 392 - 437 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for .. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r.. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | Injection |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MF003SU PP, 15% Glass Fiber Filled, Injection Molded Starpylen MF003SU is a 15% Glass Fiber Reinforced Polypropylene Injection Molding Resin (also known as Starpylen WX 15V S34/040)Information provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MF008S PP, 40% Glass Fiber Filled, Injection Molded Starpylen MF008S is a 40% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MX05038 TPEX, Injection Molded Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MX06023 PP, 20% Milled Glass Fiber Filled, Injection Molded Starpylen MX06023 is a 20% Milled Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MX06050 PP, 30% Glass Filled, Injection Molded Starpylen MX06050 is a 30% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 215 - 225 °C | 419 - 437 °F | |
Eurostar Starpylen MZ006S PP, Glass Fiber Filled, Injection Molded Starpylen MZ006S is a Glass fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WT 30GF S3)Information provided by Eurostar. |