Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 235 - 245 °C | 455 - 473 °F | |
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar. |